A start formulation about the glass flake coating based on epoxy resin:

Epoxy resin:                  30-35%
Xylene:                           10-12%
Active agent:                 3-5%
Thixotrope:                    1.2%
Pigment:                         20-15%
Glass flake(C-150E):    30-25%
Silane coupling agent: tiny
Auxiliary:                        suitable